Brief Analysis of H-703 Epoxy Adhesive Formula

Component dosage / g component dosage / g

E-51 epoxy resin 100600# epoxy thinner 10

650# polyamide 20 imidazole 8

D-17 polybutadiene epoxy resin 20β-hydroxyethyl ethylenediamine 8

Preparation and curing are weighed according to the amount, and evenly mixed. The adhesive pressure of this product is 0.07~0.15MPa. Curing at 100 ° C for 3 h or 60 ° C for 4 h.

Use This gel can be used for a long time at 100 ° C. It has excellent water and aging resistance and is used for metal and non-metal bonding.

3.0mm Vinyl Flooring is easy maintenance, essentially all you need to do to keep it clean is regularly sweep or vacuum and then damp mop with a neutral or peroxide cleaner from time to time. Tiles that have been UV cured polyurethane coating are best for ultimate longevity.

Softer surfaces of 3.0MM Vinyl Flooring are great for crawling babies, clumsy kids and people who spend a lot of time on their feet, as it reduces the pressure on the knees and joints.

3.0mm Vinyl Flooring

3.0MM Vinyl Flooring,Thick Vinyl Flooring,Waterproof Vinyl Flooring,Luxury Vinyl Plank

GreenOmni Surface Co., Ltd , https://www.greenomnifloors.com